Showing posts with label ERW carbon steel pipe. Show all posts
Showing posts with label ERW carbon steel pipe. Show all posts

2017/02/17

In Stock ERW Pipe Price 2017/02/16

 Updated Price List For In Stock ERW Steel Pipe On FEB,16,2017
API 5L/A53   GR.B, ERW Steel Pipe, Carbon Steel
Outside DiameterWall ThicknessLengthQuantity 数量Remark 标记EXW CHINA 出厂价 
外径 (mm)壁厚 (mm)长度 (mtr)PCS 根数TON 吨位Surface,EndUSD/TON 美金每吨
33.43.38 65601.40 BLACK$547.71
42.33.56 62100.71 BLACK$552.94
48.33.68 61700.69 BLACK$543.79
60.33.91 610005.44 BE. BLACK$539.87
735.16 68607.42 BE. BLACK$556.86
88.95.49 61121.26 BE. BLACK$560.78
114.35.74 61562.40 BE. BLACK$538.56
168.36.02 62405.78 BE. BLACK$545.10
2196.55 634311.77 BE. BLACK$538.56
2737.11 646621.72 BE. BLACK$545.10
33.42.9623030.10BE. BLACK$571.63
42.32.97619834.22BE. BLACK$584.71
48.33.18633070.06BEVANISH$565.10
60.33.186420112.88PE BLACK$570.33
734.786378182.38PE BLACK$567.71
88.94.786296176.10PE BLACK$567.71
114.34.786350271.10BE. BLACK$567.71
168.35.166280348.75BE. BLACK$575.56
2197.046160353.26BE. BLACK$578.17
2737.86150459.10BE. BLACK$558.56
33.42.10 63335BLACK$563.00
42.24.00 63938BLACK$566.00
48.33.25 641210BLACK$536.00
60.34.25 652117BE. BLACK$559.00
734.75 661832BE. BLACK$559.00
88.95.25 622115BE. BLACK$546.00
114.38.00 619719BE. BLACK$570.00
168.38.75 65910BE. BLACK$559.00
2199.75 610627BE. BLACK$552.00
2737.75 6228BE. BLACK$552.00
   Note:  1. The above price is based on bare pipe, for extra coating, please contact sales@primesteeltube.com;
             2. The above price is based on EXW, for FOB/CIF/CFR price, please contact sales@primesteeltube.com;
             3. The above price is not including any packing and end processing charge, for detailed quotation, please contact sales@primesteeltube.com;
             4. The above price is only valide during FEB16-  FEB23;
             5. The applicapable MOQ for this price list is over 25 tons;

2016/11/07

How to Weld for the ERW Steel Pipe in Winter

To ensure that the erw steel pipe in the winter welding perfect follow the following steps:
First, increase the welding current welding, slow down the welding speed, the appropriate increase in the cross-sectional area and length of the weld, if necessary, preheat.
Second, not outside the groove on the base metal to start arc, arc extinction to be filled when the pit.
Third, as far as possible not in low temperature conditions for bending, correction and assembly weldments.
Fourth, preheating before welding, welding process to strictly maintain the interlayer temperature should not be lower than the preheating temperature.
Fifth, the use of low hydrogen or ultra-low hydrogen welding materials.
Six, the entire weld should be finished as far as possible to avoid interruption.